Title | VANADIUM ALLOYING IN S355 STRUCTURAL STEEL: EFFECT ON RESIDUAL AUSTENITE FORMATION IN WELDED JOINTS HEAT AFFECTED ZONE |
---|---|
Publication Type | Articolo su Rivista peer-reviewed |
Year of Publication | 2022 |
Authors | Stornelli, G., Gaggiotti M., Mirabile Gattia Daniele, Schmidt R., Sgambetterra M., Tselikova A., Zucca G., and Di Schino A. |
Journal | Acta Metallurgica Slovaca |
Volume | 28 |
Pagination | 127-132 |
ISSN | 13351532 |
Abstract | The inter-critical heat affected zone (ICHAZ) appears to be one of the most brittle sections in the welding of high-strength micro-alloy steels (HSLA). Following multiple heating cycles in the temperature range between Ac1 and Ac3, the ICHAZ undergoes a strong loss of toughness and fatigue resistance, mainly caused by the formation of martensite-austenite constituent (MA). The presence of micro-alloying elements in HSLA steels induces variations in the formation of some microstructural constituents, more or less beneficial, which allow to improve the mechanical performance of a welded joint. The behavior in the inter-critical region of a S355 grade steel with 0.1wt% V addition is reported in this paper. Five double-pass welding thermal cycles were simulated using a dilatometer, with the maximum temperature of the secondary peak in the inter-critical area, in the range between 720 °C and 790 °C. The residual austenite dependence on inter-critical temperature is analyzed and related to the hardness behavior. © 2022, Technical University of Kosice. All rights reserved. |
Notes | cited By 0 |
URL | https://www.scopus.com/inward/record.uri?eid=2-s2.0-85138882584&doi=10.36547%2fams.28.3.1535&partnerID=40&md5=c8b2cd7de98a97ad37637af8b7d2f093 |
DOI | 10.36547/ams.28.3.1535 |
Citation Key | Stornelli2022127 |